1947 Chevrolet Woody Station Wagon

Before Wood Panel Refinishing:

My client had the larger wood panels replaced a few years ago on this 1947 Chevrolet Woody station wagon, but asked if I could refinish the original wood trim on his vehicle.

1947 Chevy Woody getting taped before sanding

After Wood Panel Refinishing:

We taped off the wood, and I used my FESTool sanding system to sand down all the old finish. I then used a great exterior oil based product, with a UV package added for more protection, and applied 5 coats of finish to the wood trim.
1947 Chevy Woody station wagon after wood panel refinishing

Before refinishing